How should we judge new marks on our FR5 collar samples?

NadiaCarter0987 · 16 Feb 2026, 02:57 UTC

Closed
NA
NadiaCarter0987
Our collar trial produced faint arcs on the visible surface, but two people inspected them under different lighting and disagreed. The supplier proposes softer pads. What appearance check should quality define before we compare another contact material?

4 replies

CH
ChloeBrooks0831
Replying to NadiaCarter0987

Were the arcs absent before the trial, and can you identify each collar?

4 points
NA
NadiaCarter0987
Replying to ChloeBrooks0831

We can identify them, but there are no before images and no recorded incoming appearance check. I have asked quality for judged starting samples and a consistent viewing method.

16 points
CH
ChloeBrooks0831
Replying to NadiaCarter0987

Include inspection after release, not only after holding.

20 points
OM
OmarBell0665
Replying to NadiaCarter0987

And let the normal inspector try that viewing method. The supplier needs the same acceptance reference for both pad options, alongside reliable pickup and release. Otherwise a softer material may win only because someone looked at its samples more kindly.

8 points

Discussion closed